Examples
Deburring
before

after

| Grinding Condition | |
|---|---|
| Material | ADC12 |
| S | 6000 min-1 |
| F | 1000 mm/min |
| D | 0.5 mm |
before

after

| Grinding Condition | |
|---|---|
| Material | aluminum alloy |
| S | 6000 min-1 |
| F | 1000 mm/min |
| D | 0.5 mm |
Removing tool marks
before

Ra 0.546 µm, Rz 2.169 µm
after

Ra 0.097 µm, Rz 0.441 µm
| Grinding Condition | |
|---|---|
| Material | SCM440 |
| S | 6000 min-1 |
| F | 1000 mm/min |
| D | 0.5 mm |
before

Ra 0.183 µm, Rz 0.932 µm
after

Ra 0.047 µm, Rz 0.211 µm
| Grinding Condition | |
|---|---|
| Material | SUS303 |
| S | 3000 min-1 |
| F | 800 mm/min |
| D | 0.5 mm |
before

Ra 0.785 µm, Rz 3.156 µm
after

Ra 0.265 µm, Rz 0.982 µm
| Grinding Condition | |
|---|---|
| Material | Titan |
| S | 6000 min-1 |
| F | 1000 mm/min |
| D | 0.5 mm |


SOWA Co., Ltd.